Hastelloy B-3 wrought nickel-base superalloy prices

Hastelloy B-3 wrought nickel-base superalloy prices
Hastelloy B-3 alloy is nickel molybdenum alloy as a new member of the family, Hastelloy B-3 is for any temperature and concentration of hydrochloric acid has excellent corrosion resistance.Hastelloy B-3 can be used forgings, bar, sheet, strip, ring parts, wire, bolt, spring, such as negotiating supply.

Steel grade:Hastelloy B
Equal material : UNS N10675
Alloy density:2.1 to 9.22 g/cm3
Melting point: 1418 degree
Product type : Profile steel, steel plate, steel bar
Delivery time : Promptly ( Stock) or 10-40 days (Production)
Stock : Available
MTC: Available
Payment Term : T/T or L/C At sight

Hastelloy B-3 alloy Chemical composition :

Henan Join-win Im/Ex Corp. is a professional Hastelloy B-3 superalloy steel manufacture and supplier. We stock large quality of Hastelloy B-3 superalloy steel every month. please do not hesitate to contact us.We will do service for for you at any time.

Pandora(at)steel-jw(dot)com
info(at)hastelloy-c276(dot)com
Skype: pandora.peng
Url (w)(w)(w).hastelloy-c276(dot)com
Tel:00852 2115 3188/2973

Hastelloy B-3 wrought nickel-base superalloy

Hastelloy B-3 wrought nickel-base superalloy
Hastelloy B-3 alloy is nickel molybdenum alloy as a new member of the family, Hastelloy B-3 is for any temperature and concentration of hydrochloric acid has excellent corrosion resistance.Hastelloy B-3 can be used forgings, bar, sheet, strip, ring parts, wire, bolt, spring, such as negotiating supply.

Steel grade:Hastelloy B
Equal material : UNS N10675
Alloy density:2.1 to 9.22 g/cm3
Melting point: 1418 degree
Product type : Profile steel, steel plate, steel bar
Delivery time : Promptly ( Stock) or 10-40 days (Production)
Stock : Available
MTC: Available
Payment Term : T/T or L/C At sight

Hastelloy B-3 alloy specification:

Hastelloy B-3 alloy is nickel molybdenum alloy as a new member of the family,Hastelloy B-3 is for any temperature and concentration of hydrochloric acid has excellent corrosion resistance. At the same time it to sulfuric acid, acetic acid, formic acid, phosphoric acid and other oxidizing medium also has good corrosion resistance. And, because of its chemical composition adjustment, its thermal stability compared to the original hastelloy B-2 alloy has improved significantly. To point B-3 alloy corrosion, stress corrosion cracking, corrosion and welding heat affected zone, etc all have high corrosion resistance.

Henan Join-win Im/Ex Corp. is a professional Hastelloy B-3 superalloy steel manufacture and supplier. We stock large quality of Hastelloy B-3 superalloy steel every month. please do not hesitate to contact us.We will do service for for you at any time.

Pandora(at)steel-jw(dot)com
info(at)hastelloy-c276(dot)com
Skype: pandora.peng
Url (w)(w)(w).hastelloy-c276(dot)com
Tel:00852 2115 3188/2973