Supply Hastelloy B-3 wrought nickel-base superalloy

Supply Hastelloy B-3 wrought nickel-base superalloy
Hastelloy B-3 alloy is nickel molybdenum alloy as a new member of the family, Hastelloy B-3 is for any temperature and concentration of hydrochloric acid has excellent corrosion resistance.Hastelloy B-3 can be used forgings, bar, sheet, strip, ring parts, wire, bolt, spring, such as negotiating supply.

Steel grade:Hastelloy B
Equal material : UNS N10675
Alloy density:2.1 to 9.22 g/cm3
Melting point: 1418 degree
Product type : Profile steel, steel plate, steel bar
Delivery time : Promptly ( Stock) or 10-40 days (Production)
Stock : Available
MTC: Available
Payment Term : T/T or L/C At sight

Hastelloy B-3 alloy application:

Hastelloy B-3 alloy can be used in the previous 2B is all purposes. As with B-2 alloy, B-3 is not recommended to trivalent iron salts and environment of the existence of bivalence copper salt, because these salt can quickly cause corrosion damage. When hydrochloric acid comes into contact with the iron and copper, will react to generate trivalent iron salts and bivalence copper salt.

Henan Join-win Im/Ex Corp. is a professional Hastelloy B-3 superalloy steel manufacture and supplier. We stock large quality of Hastelloy B-3 superalloy steel every month. please do not hesitate to contact us.We will do service for for you at any time.

Pandora(at)steel-jw(dot)com
info(at)hastelloy-c276(dot)com
Skype: pandora.peng
Url (w)(w)(w).hastelloy-c276(dot)com
Tel:00852 2115 3188/2973